LORD 7555

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD 7555

Main features

  • Fast A/C Handling Strength
  • Extended 45-Minute A/E Work Time
  • Non-Sag Bead Placement

Product Description

LORD 7555 Urethane Adhesive / Sealant is a bright-white, equal-mix two-component urethane system for bonding and sealing plastics and prepared metals. Its non-sag formulation holds a bead pattern and can be applied with handheld cartridges. The LORD 7555-A/C configuration provides a typical 3 to 5 minute working time and reaches handling strength in 1 hour at 77 deg F (25 deg C). The LORD 7555-A/E configuration extends working time to 45 minutes and reaches handling strength in 5 to 6 hours. Both configurations mix 1:1 by volume and can be painted immediately after application. The cured material is UV resistant and has a typical elongation of 166%.

Key features

  • Configuration-specific work times: Choose 3 to 5 minutes for LORD 7555-A/C or 45 minutes for LORD 7555-A/E at 77 deg F (25 deg C).
  • Non-sag bead control: The full-bodied formulation holds its bead pattern and resists slumping during application.
  • Immediate paintability: The applied adhesive/sealant can be painted immediately to support faster downstream processing.

Applications

Applications include bonding and sealing plastics and prepared metals, with A/C suited to smaller assemblies and A/E providing more placement time for larger projects.

Product Family

LORD 7555

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix RatioMix Ratio
1:1 by Volume

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are configuration-specific for LORD 7555-A/C and LORD 7555-A/E as identified.

PropertyValueUnitMethod / condition
Component appearanceTranslucent paste; white paste; white paste-Typical; LORD 7555-A resin; 7555-C curative; 7555-E curative
7555-A viscosity40,000 to 160,000cPTypical; resin at 77 deg F (25 deg C)
7555-C viscosity130,000 to 230,000cPTypical; curative at 77 deg F (25 deg C)
7555-E viscosity130,000 to 230,000cPTypical; curative at 77 deg F (25 deg C)
Mix ratio1:1parts by volumeTypical; LORD 7555-A/C and LORD 7555-A/E; resin to curative
Working time3 to 5; 45minutesTypical at 77 deg F (25 deg C); LORD 7555-A/C; LORD 7555-A/E
Time to handling strength1; 5 to 6hoursTypical at 77 deg F (25 deg C); LORD 7555-A/C; LORD 7555-A/E
Shelf life6monthsEach component; original unopened container at 50 to 80 deg F (10 to 27 deg C)
Technical properties

After-processing / final-state properties

Properties apply to cured LORD 7555-A/C and LORD 7555-A/E systems as identified.

PropertyValueUnitMethod / condition
Elongation166%Typical; cured LORD 7555-A/C and LORD 7555-A/E
Weathering, humidity and salt-spray resistanceResistant-Cured system; qualitative characteristic
UV resistanceResistant-Bright-white cured material; qualitative characteristic
Solvent resistanceResistant-Cured system; painting and most cleaning processes do not affect bond strength

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers