LORD 7556

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD 7556

Main features

  • Clear Plastic Bonding
  • Fast A/C Working Window
  • Non-Sag Cartridge Application

Product Description

LORD 7556-A/C Urethane Adhesive is a clear, equal-mix two-component system for bonding Lexan, ABS, polycarbonate and other supported plastics, as well as primed metals. The system combines LORD 7556-A resin with LORD 7556-C curative in 200 mL or 400 mL cartridges. The A/C system provides 4 to 6 minutes of working time at 90 deg F (32 deg C), reaches handling strength in 90 to 140 minutes at 73 deg F (23 deg C), and develops full strength after 24 hours at 77 deg F (25 deg C). Its non-sag application supports vertical and overhead placement.

Key features

  • Clear plastic-bonding system: Bonds supported plastics including Lexan, ABS and polycarbonate, plus properly prepared metals.
  • Fast A/C processing window: Provides 4 to 6 minutes of working time and 90 to 140 minutes to handling strength at the stated temperatures.
  • Non-sag cartridge application: Equal-volume cartridges dispense the A/C system for placement on vertical or overhead surfaces.

Applications

Applications include sign assembly and bonding supported plastics, polycarbonate, prefinished or primed metals, and other supported substrates.

Product Family

LORD 7556

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Translucent Paste
Mix RatioMix Ratio
1:1 by Volume

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system values apply specifically to the LORD 7556-A/C configuration.

PropertyValueUnitMethod / condition
Component appearanceTranslucent paste; translucent paste-Typical; LORD 7556-A resin; LORD 7556-C curative
Component viscosity40,000 to 160,000; 80,000 to 300,000cPTypical at 77 deg F (25 deg C); LORD 7556-A resin; LORD 7556-C curative
Component density9.64 to 10.04; 9.2 to 9.6lb/galTypical; LORD 7556-A resin; LORD 7556-C curative
Mix ratio1:1parts by volumeLORD 7556-A resin to LORD 7556-C curative
Working time4 to 6minutesTypical; LORD 7556-A/C at 90 deg F (32 deg C)
Time to handling strength90 to 140minutesTypical; LORD 7556-A/C at 73 deg F (23 deg C)
Shelf life6monthsOriginal unopened container at 70 to 80 deg F (21 to 27 deg C)
Technical properties

After-processing / final-state properties

Qualitative resistance properties apply to the cured LORD 7556-A/C adhesive system.

PropertyValueUnitMethod / condition
Weathering, humidity and salt-spray resistanceResistant-Cured LORD 7556-A/C system; qualitative characteristic
UV resistanceResistant-Cured LORD 7556-A/C system; qualitative characteristic
Solvent resistanceResistant-Cured LORD 7556-A/C system; painting and most cleaning processes do not affect bond strength

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers