LORD RT8

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD RT8

Main features

  • 800 to 1000 cP Flowability
  • Low-Exotherm Potting Systems
  • Large-Casting Encapsulation Fit

Product Description

LORD RT-8 Hardener is a green, modified tertiary amine component for supported LORD epoxy potting and encapsulation systems. This legacy hardener has a typical viscosity of 800 to 1000 cP and specific gravity of 0.99 at 25 deg C. Within compatible systems, the hardener is used for low-exotherm, semirigid potting, including large castings. RT-8 is a hardener component; its properties do not represent those of a complete cured epoxy system. Current commercial status and exact RT-8 safety documentation require confirmation.

Key features

  • Flowable hardener viscosity: Provides a typical 800 to 1000 cP component viscosity at 25 deg C.
  • Low-exotherm system behavior: Supports low-exotherm, semirigid behavior when used in the specified compatible epoxy systems.
  • Large-casting encapsulation fit: RT-8 is used for potting and encapsulation of large castings in compatible systems.

Applications

Applications include use as the hardener component in supported LORD epoxy potting and encapsulation systems, including large castings within the specified compatible systems.

Product Family

LORD RT8

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
ViscosityViscosity
800-1000 mPa.s
General Properties
Chemistry TypeChemistry Type
Modified tertiary amine
ColorColor
Green
Specific GravitySpecific Gravity
0.99

Additional Information

Technical properties

As-supplied / before-processing properties

Only exact RT-8 component properties are shown; complete-system cured values are not transferred to this standalone hardener page.

PropertyValueUnitMethod / condition
Component roleEpoxy hardener-Standalone LORD RT-8 component
Hardener typeModified tertiary amine-Manufacturer technical bulletin
ColorGreen-Typical; as supplied
Viscosity800 to 1000cPTypical at 25 deg C
Specific gravity0.99-Typical at 25 deg C
Shelf life1yearFrom date of shipment in unopened containers; bulletin-wide storage statement

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers