MOLYKOTE 7375

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 7375

Main features

  • Multipurpose Brake-Pad Addition
  • 3 to 7 Weight-Percent Blending
  • Up to 650 deg C Application

Product Description

MOLYKOTE 7375 Lubolid Additive Powder is a free-flowing gray blend of inorganic solids used as a multipurpose additive in friction-lining formulations. Passenger-car and railroad brake pads are the main applications, while other supported Lubolid applications include disc, drum, rail, industrial brake and clutch linings. The powder may be added at a recommended 3 to 7 weight percent and mixed to homogeneous distribution. Its application-temperature limit is 650 deg C. Grade-specific properties include 0.74 g/cm3 tamped density, 3.1% residue on a 100 micron screen and 1.0% maximum moisture; these are additive properties, not finished-brake performance ratings.

Key features

  • Multipurpose brake-pad addition: Supports passenger-car and railroad brake-pad formulations as the main applications.
  • 3 to 7 weight-percent blending: Add within this recommended range, then mix to homogeneous distribution.
  • Up to 650 deg C application: Has this maximum application temperature for supported friction-lining formulations.

Applications

Passenger-car and railroad brake pads are the main applications, with additional supported use in disc, drum, rail, industrial brake and clutch lining formulations.

Product Family

MOLYKOTE 7375

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Gray

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values are exact to MOLYKOTE 7375 Lubolid Additive Powder.

PropertyValueUnitMethod / condition
ColorGray-Typical; as supplied
ConsistencyFree-flowing powder-Typical; as supplied
Tamped volume135ml/100 gTypical; exact 7375 grade
Tamped density0.74g/cm3Typical; exact 7375 grade
Theoretical density3.26g/cm3Typical; exact 7375 grade
Residue on 100 micron screen3.1%Typical; exact 7375 grade
Moisture1.0 maximum%Typical; exact 7375 grade
Usable life60monthsOriginal unopened bag at or below 25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers