MOLYKOTE PG21

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE PG21

Main features

  • Wide-Temperature Plastic Lubrication
  • Oxidation-Resistant Silicone Grease
  • Water-Resistant Friction Contact Lubrication

Product Description

MOLYKOTE PG-21 Plastislip Grease is a silicone-oil grease with a lithium-complex thickener for plastic/plastic and plastic/metal friction contacts under light to medium loads and slow to medium-fast movement. The white NLGI 2 grease has a -50 to 190 deg C service range. Typical tests give a 0.1 bar oxidation pressure drop after 100 hours at 99 deg C and corrosion degree 0. It can be applied by brush, spatula, grease gun, automatic lubricating device, or central lubrication system. Applications include control cables, water pumps, bearing bushes, gearwheels, slideways, and plastic parts in domestic, toy, and electrical equipment.

Key features

  • Wide Service-Temperature Range: The typical service range extends from -50 to 190 deg C.
  • Plastic Friction Contacts: The grease is intended for plastic/plastic and plastic/metal contacts under light to medium loads.
  • Oxidation and Corrosion Performance: Typical oxidation pressure drop is 0.1 bar and corrosion degree is 0 under the specified test methods.

Applications

Control cables, water pumps, bearing bushes, gearwheels, slideways, and plastic friction contacts in domestic, toy, and electrical equipment.

Product Family

MOLYKOTE PG21

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
White
Density (g)Density (g)
0.96 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorWhite-Typical value
NLGI consistency class2UnitlessDIN 51818; typical value
Worked penetration265 to 295mm/10ISO 2137; typical value
Density0.96g/mlISO 2811; 20 deg C; typical value
Dropping point250deg CISO 2176; typical test result; not a service-temperature limit

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers