MOLYKOTE YM102

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE YM102

Main features

  • Mixed-Material Sliding Lubrication
  • Wide-Temperature PAO Grease
  • Low-Seepage Precision Equipment Use

Product Description

MOLYKOTE YM-102 Grease is a PAO-based lithium grease with solid lubricants for plastic and mixed-material sliding contacts. The yellow grease has an NLGI 1 to 2 consistency, and its base oil measures 29 mm^2/s at 40 deg C. Low and high temperature limits are -50 and 150 deg C. The grease offers load-carrying capability, wear resistance, long service life, and low seepage where cleanliness matters. Applications include plastic/plastic, metal/metal, and plastic/metal friction parts in automobiles, electrical appliances, precision equipment, and office equipment.

Key features

  • Mixed-Material Sliding Contacts: The grease is used for plastic/plastic, metal/metal, and plastic/metal friction parts.
  • Wide Temperature Range: Low and high temperature limits are -50 and 150 deg C.
  • Low-Seepage Clean Lubrication: Low seepage supports use where lubricant cleanliness is important.

Applications

Automobiles, electrical appliances, precision equipment, and office equipment with plastic/plastic, metal/metal, or plastic/metal sliding contacts.

Product Family

MOLYKOTE YM102

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Yellow
Density (g)Density (g)
0.91 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorYellow-Product detail
NLGI grade1 to 2UnitlessProduct detail
Base-oil viscosity29mm^2/s40 deg C; product detail
ThickenerLithium-Product detail

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers