PERMABOND 4C10
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

Main features
- Low-Viscosity Fine-Gap Bonding
- Fast 5-20 Second Fixture
- Hard-to-Bond Rubber Adhesion
Product Description
PERMABOND 4C10 is a low-viscosity ethyl cyanoacrylate adhesive for rapid bonding of plastics and elastomers, including hard-to-bond natural rubber, EPDM, and butyl rubber. Typical viscosity is 30 to 50 mPa s at 25 deg C, supporting thin bondlines and a maximum gap fill of 0.1 mm. Fixture times are typically 5 to 10 seconds on Buna N rubber, phenolic, PVC, and ABS, with steel reaching fixture strength in 10 to 15 seconds. The cured adhesive also provides measured shear strength on steel, aluminum, zinc, and selected engineering plastics.
Key features
- Low-Viscosity Fine-Gap Bonding: Typical viscosity of 30 to 50 mPa s supports a maximum gap of 0.1 mm.
- Fast Multi-Substrate Fixture: Fixture strength is typically reached within 5 to 20 seconds across the specified rubber, plastic, and steel substrates.
- Hard-to-Bond Rubber Capability: The grade is specified for natural rubber, EPDM, butyl rubber, and hard-to-bond plastics.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
AppearanceAppearance
ColourlessChemistry TypeChemistry Type
Ethyl cyanoacrylateSpecific GravitySpecific Gravity
1.1Physical Properties
ViscosityViscosity
30-50 mPa.sAdditional Information
Technical properties
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | - | Typical as supplied |
| Appearance | Colourless | - | Typical as supplied |
| Viscosity | 30 to 50 | mPa s | Typical at 25 deg C |
| Specific gravity | 1.1 | - | Typical |
| Maximum gap fill | 0.1 | mm | Typical curing property |
| Fixture / handling time - steel | 10 to 15 | seconds | 0.3 N/mm^2 shear strength |
Technical properties
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength - steel | 18 to 22 | N/mm^2 | ISO 4587; typical |
| Shear strength - aluminium | 6 to 8 | N/mm^2 | ISO 4587; typical |
| Impact strength | 3 to 5 | kJ/m^2 | ASTM D-950; typical |
| Dielectric strength | 25 | kV/mm | Typical cured adhesive |
| Hardness | 85 | Shore D | ISO 868; typical |