PERMABOND 4C30

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

PERMABOND 4C30

Main features

  • 0.38 mm Gap Bonding
  • Fast 15-Second Fixture
  • Automated Assembly Dispensing Capability

Product Description

PERMABOND 4C30 is an intermediate-viscosity ethyl cyanoacrylate adhesive for rapid bonding across small-to-intermediate gaps. Typical viscosity is 1200 to 2400 mPa s at 25 deg C, with a maximum gap fill of 0.38 mm and typical 15-second fixture time on steel, Buna N rubber, and phenolic. The grade is suitable for plastics, rubber, and metals and can be dispensed automatically, combining controlled flow with fast room-temperature cure. Typical cured steel shear strength is 20 to 22 N/mm^2.

Key features

  • Intermediate-Viscosity Gap Bonding: A typical viscosity of 1200 to 2400 mPa s supports gaps up to 0.38 mm.
  • 15-Second Fixture: Steel, Buna N rubber, and phenolic typically reach fixture strength in 15 seconds.
  • Automated Dispensing Fit: The grade can be dispensed automatically in fast assembly processes.
Product Family

PERMABOND 4C30

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
1200-2400 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionEthyl cyanoacrylate-Typical as supplied
AppearanceColourless-Typical as supplied
Viscosity1200 to 2400mPa sTypical at 25 deg C
Specific gravity1.1-Typical
Maximum gap fill0.38mmTypical curing property
Fixture / handling time15secondsTypical on steel at 0.3 N/mm^2 shear strength
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shear strength - steel20 to 22N/mm^2ISO 4587; typical
Impact strength3 to 5kJ/m^2ASTM D-950; typical
Dielectric strength25kV/mmTypical cured adhesive
Thermal conductivity0.1W/(m K)Typical cured adhesive
Hardness85Shore DISO 868; typical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers