PERMABOND 791

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

PERMABOND 791

Main features

  • Ultra-Fast 2-3 Second Fixture
  • Surface-Insensitive Porous Surface Bonding
  • Reduced Frosting and Fogging

Product Description

PERMABOND 791 is a low-viscosity, surface-insensitive ethyl cyanoacrylate adhesive for very fast bonding of difficult, acidic, or porous surfaces. It is particularly suited to wood and plated surfaces while also bonding plastics, metals, ceramics, and elastomers. Typical viscosity is 15 to 50 mPa s at 25 deg C with a maximum gap fill of 0.1 mm. Steel, Buna N rubber, and phenolic can reach fixture strength in 2 to 3 seconds. The rapid cure also minimizes frosting and fogging, making the grade useful where both speed and a cleaner visible bond area matter.

Key features

  • 2-3 Second Fixture: Steel, Buna N rubber, and phenolic typically reach fixture strength in 2 to 3 seconds.
  • Surface-Insensitive Bonding: The adhesive rapidly bonds acidic and porous surfaces such as wood and plated substrates.
  • Reduced Frosting and Fogging: The fast cure minimizes frosting and fogging around the bonded area.

Applications

Bonding wood, porous or acidic surfaces, plated surfaces, plastics, metals, ceramics, and elastomers.

Product Family

PERMABOND 791

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
15-50 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionEthyl cyanoacrylate-Typical as supplied
AppearanceColourless-Typical as supplied
Viscosity15 to 50mPa sTypical at 25 deg C
Specific gravity1.1-Typical
Maximum gap fill0.1mmTypical curing property
Fixture / handling time2 to 3secondsTypical on steel at 0.3 N/mm^2 shear strength
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shear strength - steel18 to 22N/mm^2ISO 4587; typical
Tensile strength>20N/mm^2ISO 6922; typical
Thermal conductivity0.1W/(m K)Typical cured adhesive
Dielectric strength25kV/mmTypical cured adhesive
Hardness85Shore DISO 868; typical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers