PERMABOND 802

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

PERMABOND 802

Main features

  • High-Temperature Bonding Performance
  • Low-Viscosity 0.15 mm Gap Bonding
  • Fast 10-15 Second Fixture

Product Description

PERMABOND 802 is a low-viscosity modified ethyl cyanoacrylate adhesive for fast bonding where high-temperature resistance is required. Typical viscosity is 90 to 110 mPa s at 25 deg C and the maximum gap fill is 0.15 mm, giving more gap capability than an ultra-thin instant adhesive while retaining rapid cure. Steel, Buna N rubber, and phenolic typically reach fixture strength in 10 to 15 seconds, and full strength develops in 24 hours. The grade bonds rubber, metals, and plastics and provides typical steel shear strength of 19 to 23 N/mm^2 after cure.

Key features

  • High-Temperature Bonding Grade: The modified cyanoacrylate is formulated for applications requiring high-temperature resistance.
  • 0.15 mm Gap Capability: Typical viscosity of 90 to 110 mPa s supports a maximum gap of 0.15 mm.
  • 10-15 Second Fixture: Steel, Buna N rubber, and phenolic typically reach fixture strength in 10 to 15 seconds.

Applications

Bonding rubber, metals, and plastics in elevated-temperature service.

Product Family

PERMABOND 802

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
90-110 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionEthyl cyanoacrylate-Typical as supplied
AppearanceColourless-Typical as supplied
Viscosity90 to 110mPa sTypical at 25 deg C
Specific gravity1.1-Typical
Maximum gap fill0.15mmTypical curing property
Fixture / handling time10 to 15secondsTypical on steel at 0.3 N/mm^2 shear strength
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shear strength - steel19 to 23N/mm^2ISO 4587; typical
Shear strength - polycarbonate6N/mm^2ISO 4587; typical
Thermal conductivity0.1W/(m K)Typical cured adhesive
Dielectric strength25kV/mmTypical cured adhesive
Hardness85Shore DISO 868; typical
Minimum stated exposure temperature-55deg CDepends on materials being bonded

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers