PERMABOND ET500

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET500

Main features

  • 5 to 8 Minute Handling
  • Clear Rapid-Cure Epoxy Bonding
  • 12 to 18 MPa Shear

Product Description

PERMABOND ET500 is a clear, two-component epoxy adhesive for rapid structural assembly. Viscosity is 13,000 to 24,000 mPa s, handling time is 5 to 8 minutes at 23 deg C, and shear strength is 12 to 18 MPa. The fast handling profile suits smaller or time-sensitive bonding operations where a clear epoxy is preferred. Applications include bonding wood, metals, ceramics, selected plastics and composites. The resin-and-hardener format provides a structural epoxy bond for multi-material joints while keeping the assembly window short enough for rapid production steps and quick transition from placement to handling.

Key features

  • 5 to 8 Minute Handling: Handling time is 5 to 8 minutes at 23 deg C for rapid assembly workflows.
  • Clear Two-Part Epoxy: The product is a clear epoxy resin and hardener system for structural bonding.
  • 12 to 18 MPa Shear: Shear strength is 12 to 18 MPa.

Applications

Bonding wood, metals, ceramics, selected plastics and composites in small or rapid assembly applications.

Product Family

PERMABOND ET500

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless
Chemistry TypeChemistry Type
Epoxy Resin/Amine Hardener
Mix RatioMix Ratio
1:1
Specific GravitySpecific Gravity
1.1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
12,000-18,000 mPa.s
Viscosity (Part B)Viscosity (Part B)
15,000-30,000 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
15-25 kV/mm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.22 W/m.K

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers