PERMABOND ET510

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET510

Main features

  • 20 to 40 Minute Handling
  • Flexible Impact-and-Peel Positioning
  • Rapid Multi-Material Structural Bonding

Product Description

PERMABOND ET510 is a rapid-curing, flexible two-component epoxy adhesive for structural bonding where impact and peel behavior are important. Viscosity is 22,000 to 39,000 mPa s, handling time is 20 to 40 minutes at 23 deg C, and shear strength is 8 to 12 MPa. The handling window provides time for component placement while remaining suited to relatively quick assembly. Applications include bonding wood, metals, ceramics, selected plastics and composites where relatively fast handling is required. Its flexible cured profile is useful for joints where peel and impact behavior are important to the joint design.

Key features

  • 20 to 40 Minute Handling: Handling time at 23 deg C balances assembly time with relatively fast processing.
  • Flexible Epoxy Profile: The flexible cured profile is intended for structural joints where impact and peel resistance are important.
  • 8 to 12 MPa Shear: Shear strength is 8 to 12 MPa.

Applications

Bonding wood, metals, ceramics, selected plastics and composites where relatively fast handling is required.

Product Family

PERMABOND ET510

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless/Amber
Chemistry TypeChemistry Type
Epoxy Resin/Polyamine Hardener
Specific GravitySpecific Gravity
1.1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
14,000-28,000 mPa.s
Viscosity (Part B)Viscosity (Part B)
30,000-50,000 mPa.s
Mechanical Properties
ElongationElongation
15-25 %
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
40-50 °C
Thermal ConductivityThermal Conductivity
0.35 W/m.K
Electrical Properties
Dielectric StrengthDielectric Strength
15-25 kV/mm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers