Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET5401

Main features

  • Thixotropic Gap-Filling Paste
  • 60 to 90 Minute Handling
  • High-Temperature Structural Bonding

Product Description

PERMABOND ET5401 is a toughened, thixotropic two-component epoxy adhesive for structural bonding, gap filling and elevated-temperature applications. It is supplied as a thick paste, with a handling time of 60 to 90 minutes at 23 deg C and shear strength of 20 to 30 MPa. The non-slump, flow-control character is suited to vertical or gap-filling joints where adhesive placement must be maintained during assembly. Applications include bonding wood, metals, ceramics, selected plastics and composites where high-temperature resistance and gap filling are required. Its paste rheology and intermediate handling window make it useful for structural assembly geometries that need controlled adhesive placement.

Key features

  • Thick Thixotropic Paste: Non-slump flow control is suited to vertical and gap-filling structural joints.
  • 60 to 90 Minute Handling: Handling time at 23 deg C provides an intermediate assembly window.
  • 20 to 30 MPa Shear: Shear strength is 20 to 30 MPa.

Applications

Structural bonding of wood, metals, ceramics, selected plastics and composites where high-temperature resistance and gap filling are required.

Product Family

PERMABOND ET5401

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
White/Black
Chemistry TypeChemistry Type
Epoxy Resin/Polyamine Hardener
Specific GravitySpecific Gravity
1.2/1.1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
60,000 120,000 mPa.s
Viscosity (Part B)Viscosity (Part B)
50,000 100,000 mPa.s
Mechanical Properties
ElongationElongation
4 - 8 %
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
50 - 110 °C
Electrical Properties
Dielectric StrengthDielectric Strength
15 - 25 kV/mm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers