PERMATEX 133-K

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

PERMATEX 133-K

Main features

  • Aluminum-Copper-Graphite Anti-Seize Blend
  • Service to 870 deg C
  • Meets MIL-A-907E Requirements

Product Description

Permatex Anti-Seize Lubricant, 8 oz is a heavy-duty anti-seize lubricant containing aluminum, copper and graphite lubricating solids for high-temperature threaded and slow-moving assemblies. The metallic paste has a typical viscosity of 100,000-200,000 cP and a specific gravity of 1.13. Its stated service range extends from -51 to 870 deg C. The lubricant is used to reduce galling, seizing and wear under heavy contact pressure while supporting later disassembly of heat-exposed or corrosive assemblies. The product meets or exceeds the requirements of MIL-A-907E and is not intended for wheel lug nut or stud applications.

Key features

  • Aluminum, copper and graphite anti-seize: The lubricating-solid blend is formulated for threaded and slow-moving assemblies exposed to heat and pressure.
  • Service range to 870 deg C: The stated temperature range is -51 to 870 deg C.
  • MIL-A-907E requirement: The product meets or exceeds the requirements of Military Specification MIL-A-907E.

Applications

Spark-plug threads; exhaust-manifold and engine bolts; brake anchor pins; U-bolts and spring bolts; hinges, gears, chains, sprockets and rollers; boiler and oven parts.

Product Family

PERMATEX 133-K

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Silver metallic past
Chemistry TypeChemistry Type
Grease
Specific GravitySpecific Gravity
1.13
Thermal Properties
Operating TemperatureOperating Temperature
-60 - 870 °C
Physical Properties
ViscosityViscosity
1000000 - 2000000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical typeGrease-As supplied
Lubricating solidsAluminum, copper and graphite-As supplied
Specific gravity1.13-As supplied
Viscosity100,000-200,000cPAs supplied
Flash point>350deg FAs supplied

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers