PLEXUS MA2245

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PLEXUS MA2245

Main features

  • 40-42, 50 or 106 Minute Work Times
  • Highly Thixotropic 10:1 Adhesive Family
  • 0.75-38 mm Grade-Specific Gaps

Product Description

Plexus MA2245 is highly thixotropic two-part methacrylate structural adhesives for thermoplastic, metal and composite assemblies. Each grade uses a 10:1 mix ratio and retains its own processing and cured-property data. At 23.9 deg C, typical work time is50 minutes for MA2245. All three grades list gap tolerance from 0.75 to 38 mm.

Key features

  • Three grade-specific work-time options: At 23.9 deg C, MA2245 is 50 minutes
  • 10:1 two-part methacrylate systems
  • 0.75-38 mm grade-specific gap tolerance: Each grade lists a gap tolerance of 0.75 to 38 mm in its own technical data.

Applications

Structural bonding of composites, thermoplastics and metals; large-bead and vertical assemblies where the selected grade's work time and technical data support use.

Product Family

PLEXUS MA2245

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White/Black
Density (g)Density (g)
0.99/1.07 g/cm3
Mix RatioMix Ratio
10:1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
190 - 250 mPa.s
Viscosity (Part B)Viscosity (Part B)
35 - 70 mPa.s
Mechanical Properties
ElongationElongation
40 - 80 %

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers