LOCTITE STYCAST PC40-UMF

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE STYCAST PC40-UMF

Main features

  • VOC free
  • Single component
  • UV and Moisture cure

Product Description

LOCTITE® STYCAST PC 40-UMF conformal coating is specifically formulated to rapidly gel and immobilize when exposed to UV light and then fully cure when exposed to atmospheric moisture, ensuring optimum performance even in shadowed areas.

LOCTITE STYCAST PC 40-UMF offers very low outgassing and CVCM content that conforms to IPC-CC-830 requirements. It is a great product for multiple substrates, including a variety of metal surfaces, ceramic, and glass filled epoxy.

Advantages of Loctite Stycast PC 40-UMF

  • Single Component
  • VOC free
  • UV and moisture curable

Cure Schedule

  • 10 seconds @ 300 to 600 mW/cm² UV
  • Wavelength, nm 365
Product Family

STYCAST PC40-UMF

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 15 days
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.08
Thermal Properties
Thermal ConductivityThermal Conductivity
0.26 W/m.K
Electrical Properties
Dielectric StrengthDielectric Strength
16.5 kV/mm
Surface ResistivitySurface Resistivity
3.8x10^16 Ohms/sq
Volume ResistivityVolume Resistivity
350000000000000000 Ohms⋅cm
Physical Properties
ViscosityViscosity
250 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers