TECHNOMELT 1942
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- 30-Second Assembly Open Time
- Wood and Multi-Plastic Bonding
- High-Elongation Hot-Melt Performance
Product Description
TECHNOMELT 1942 is an EVA-based, medium-setting hot-melt adhesive for general-purpose bonding of wood and plastics including nylon, polycarbonate, PVC, polystyrene, ABS, and acrylic. The one-part material has a typical viscosity of 5,000 cP at 350 deg F, a 30-second open time, and a 198 deg F softening point. Typical material data include 250 psi tensile strength, 500% elongation, and dielectric strength above 1,100 V/mil. This balance of open time, substrate range, and material properties suits general-purpose wood and plastic bonding.
Key features
- Thirty-second open time: Typical open time is 30 seconds for prompt part assembly.
- Wood and plastic adhesion: The adhesive bonds wood and multiple engineering and commodity plastics.
- High elongation: Typical elongation is 500% by ASTM D638.
Applications
Bonding wood, nylon, polycarbonate, PVC, polystyrene, ABS, acrylic, and other supported substrates.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Values are typical product-selection data and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Softening point | 198 | deg F | ASTM E28-67; typical |
| Viscosity | 5,000 | cP | 350 deg F; ASTM D3236; typical |
| Open time | 30 | sec | Typical |
| Specific gravity | 0.96 | 77 deg F; ASTM D792; typical |
After-processing / final-state properties
Values describe the cured material and are typical product-selection data, not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Heat resistance | 142 | deg F | ASTM D4498; typical |
| Tensile strength | 250 | psi | ASTM D638; typical |
| Elongation | 500 | % | ASTM D638; typical |
| Glass transition temperature | 7 | deg F | ASTM E1640; typical |
| Dielectric strength | Above 1,100 | V/mil | ASTM D149; typical |