3M DP8825NS

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M DP8825NS

Main features

  • 3,000 psi Typical 7-Day Aluminum Overlap Shear
  • 22 to 24-Minute Work Life
  • 0.010-Inch Glass-Bead Control

Product Description

3M Scotch-Weld Low Odor Acrylic Adhesive DP8825NS is a low-odor, non-sag two-part acrylic adhesive for bonding metals and plastics, including slightly oily surfaces. It mixes 10:1 by volume and weight and contains 0.010-inch glass beads for bondline control. Typical work life is 22 to 24 minutes at 23 deg C. At 22 deg C, typical open time is 21 minutes, and structural strength of 6.9 MPa overlap shear develops in 50 to 56 minutes. Typical full cure takes 24 hours at 23 deg C to reach at least 80% of ultimate aluminum overlap shear. Typical aluminum overlap shear is 3,000 psi after seven days at 23 deg C with light abrasion, solvent cleaning, and a 0.25 mm bondline.

Key features

  • 22 to 24-minute work life: The typical maximum static-mixer residence interval applies at 23 deg C; typical open time before bond closure is 21 minutes at 22 deg C.
  • 0.010-inch glass beads: The embedded beads control spacing between bonded surfaces.
  • 3,000 psi aluminum overlap shear: Typical strength follows seven days at 23 deg C, light abrasion and solvent cleaning, and a 0.25 mm bondline under ASTM D1002/ISO 4587.

Applications

HVAC, appliance, sporting-goods, specialty-vehicle, and sign-manufacturing assemblies; bonding plastics, composites, and powder coats to metal.

Product Family

3M DP8825NS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Blue-Green
Component SystemComponent System
Two (Accelerator | Base)
Physical Properties
Open timeOpen time
21 minutes
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical and not specifications.

PropertyValueUnitMethod / condition
Mix ratio by volume (B:A)10:1-Two-part system
Mix ratio by weight (B:A)10:1-Two-part system
Base viscosity40,000cP23 deg C; cone-and-plate
Accelerator viscosity15,000cP23 deg C; cone-and-plate
Mixed viscosity40,000cPTypical value
Open time21minMaximum before bond closure and fixing
Work life22 to 24min23 deg C; static mixing nozzle
Time to structural strength50 to 56minTime to 6.9 MPa overlap shear

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers