EPOCAST 52

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

EPOCAST 52

Main features

  • Graphite Composite Laminating
  • 66 to 93 deg C Vacuum-Bag Cure
  • 177 deg C Maximum Service Temperature

Product Description

EPOCAST 52 A/B is a two-part epoxy laminating system for fabrication and repair of graphite composites. The blue Part A resin and straw-colored Part B hardener mix at 100:41 by weight or 2:1 by volume, producing an amber material with typical viscosity of 5,500 cP at 25 deg C. The system supports low-temperature vacuum-bag curing, good wetting, and hot-wet strength, with service capability up to 177 deg C. Typical cure cycles are three hours at 66 deg C or two hours at 93 deg C. Qualifications include AIMS 08-01-002-01, AIMS 08-02-002-01, and SAE AMS2980.

Key features

  • Graphite Composite Laminating: The epoxy system is formulated for fabrication and repair of graphite composite structures.
  • Low-Temperature Vacuum-Bag Cure: Typical cure cycles are three hours at 66 deg C or two hours at 93 deg C.
  • Maximum Service Temperature: Maximum service temperature is 177 deg C within the stated hot-wet performance context.

Applications

Graphite-composite fabrication; composite repair; laminating; low-temperature vacuum-bag processing.

Product Family

EPOCAST 52

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Amber
Component SystemComponent System
Two Part (Resin | Hardener)
Density (g)Density (g)
1.10 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical Part A, Part B, and mixed-system properties from the exact Huntsman TDS.

PropertyValueUnitMethod / condition
AppearanceBlue / straw / amber-Part A / Part B / mixed system; visual
Density1.20 / 1.00 / 1.10g/cm3Part A / Part B / mixed system; ASTM D792
Viscosity14,000 / 1,500 / 5,500cPPart A / Part B / mixed system; 25 deg C; ASTM D2196
Mix ratio100:41parts by weightPart A resin:Part B hardener
Mix ratio2:1parts by volumePart A resin:Part B hardener
Gel time3.5 to 5.5hoursMixed system; 100 g at 25 deg C
Shelf life1yearOriginal sealed containers at 2 to 8 deg C
Technical properties

After-processing / final-state properties

Typical laminate-system values with the stated cure and conditioning context; samples used 36% resin content on T300 3KPW.

PropertyValueUnitMethod / condition
Maximum service temperature177deg CTypical system value after either listed cure
Short-beam shear strength7.7KsiAt 25 deg C; 93 deg C cure
Wet short-beam shear strength7.4KsiAt 80 deg C after stated wet conditioning; 93 deg C cure
Wet tensile strength18KsiAt 71 deg C after stated wet conditioning; 93 deg C cure
Compression interlaminar shear8.6KsiAt 25 deg C; 93 deg C cure
Glass transition temperature133deg CAfter 3 hours at 66 deg C
Glass transition temperature155deg CAfter 3 hours at 66 deg C plus 1 hour at 177 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers