LOCTITE 392

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE 392

Main features

  • Rapid Activator-Cure Assembly
  • Tough Impact and Peel Resistance
  • DC Motor Magnet Bonding

Product Description

LOCTITE AA 392 is a one-part modified acrylic structural adhesive used with separately applied LOCTITE Activator 7380 or 7387. The medium-viscosity material is suited to fast assembly, including DC motor magnet bonding and pre-coated sheet-metal joining. On steel with Activator 7380, fixture time is <=25 seconds at a 0.05 mm gap; the recommended bondline gap is 0.1 mm. The cured adhesive has Shore D 65 hardness, 130% elongation, and strong impact and peel performance for assembly lines with short cycle times. The activator is applied separately and is not included with the adhesive.

Key features

  • Rapid Activator Cure: Fixture time is <=25 seconds on steel at a 0.05 mm gap.
  • Tough Impact and Peel Performance: The cured adhesive combines impact resistance with peel resistance.
  • Motor Magnet Assembly Fit: The product is used for DC motor and magnet bonding.

Applications

Applications include DC motor magnet bonding and pre-coated sheet-metal assembly.

Product Family

LOCTITE 392

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Translucent beige to dark amber
Chemistry TypeChemistry Type
Modified acrylic
Specific GravitySpecific Gravity
1.16
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C
Electrical Properties
Volume ResistivityVolume Resistivity
1.8×10¹⁵ Ohms⋅cm
Physical Properties
ViscosityViscosity
6,500 to 17,500 mPa.s
Mechanical Properties
ElongationElongation
130 %

Additional Information

Technical properties

As-Supplied Properties

PropertyValueUnitMethod / condition
AppearanceTranslucent beige to dark amber-Uncured
Specific gravity1.16-25 deg C
Viscosity20,000 to 80,000mPa sBrookfield HBT, spindle TA, 2.5 rpm, helipath, 25 deg C
Viscosity6,500 to 17,500mPa sBrookfield HBT, spindle TA, 20 rpm, helipath, 25 deg C
Technical properties

Final-State Properties

PropertyValueUnitMethod / condition
Hardness65Shore DISO 868
Elongation130%ISO 527-3
Tensile strength18.6N/mm^2ISO 527-3
Tensile modulus144.8N/mm^2ISO 527-3
Lap shear strength>=11.7N/mm^2Steel; 24 h at 22 deg C; Activator 7380 on one side
Lap shear strength11N/mm^2Aluminum; 48 h at 22 deg C; Activator 7380 on one side

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers