LOCTITE AA 312

Harmonization Code : 3506.10.5000 | HTS - Other Products Suitable For Use As Glues, Put Up For Retail Sale As Glues, Not Exceeding A Net Weight Of 1 Kg

LOCTITE AA 312

Main features

  • One-Component Formulation
  • Room-Temperature Cure
  • Dissimilar Material Bonding

Product Description

LOCTITE® AA 312™ is a one-component modified acrylic ester adhesive formulated for bonding dissimilar materials, including metals, glass, and ceramics. Used with LOCTITE® Activator 736™ or 734™, the adhesive cures at room temperature and provides rapid fixture times for close-fitting assemblies. Its medium-viscosity formulation requires no mixing, making it suitable for manufacturing and industrial bonding applications where fast processing and reliable bond development are required.

Key features

  • One-component formulation: Requires no mixing, simplifying application and assembly processes.
  • Room-temperature cure: Cures with LOCTITE® Activator 736™ or 734™ to support rapid fixture times.
  • Dissimilar material bonding: Suitable for bonding metals, glass, and ceramics in close-fitting assemblies.

Applications / Suitable for

  • Metal-to-metal bonding
  • Glass bonding applications
  • Ceramic assembly applications
  • Industrial manufacturing and assembly operations
  • Close-fitting bonded joints requiring fast fixturing
Product Family

LOCTITE AA 312

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of LOCTITE® AA 312™ before curing and assembly.

Property Value Unit Method / condition
Chemical Type Modified acrylic ester - As supplied
Appearance Clear amber liquid - Uncured material
Specific Gravity 1.1 - 25°C
Viscosity 850-1,200 mPa·s (cP) Brookfield RVT, Spindle 2, 20 rpm, 25°C
Technical properties

After-processing / final-state properties

Typical cured-material properties and lap shear strength performance data.

Property Value Unit Method / condition
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/(m·K) ISO 8302
Specific Heat 0.3 kJ/(kg·K) Cured material
Lap Shear Strength ≥17.2 N/mm² ISO 4587, steel (grit blasted), 24 h @ 22°C, Activator 736™ or 734™ on 2 sides

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers