Main features

  • High-Viscosity Magnet Bonding
  • Fast Activator-Assisted Fixture
  • Impact- and Peel-Resistant Bonds

Product Description

LOCTITE AA 332 is a one-component, high-viscosity modified acrylic structural adhesive developed for metal and permanent-magnet bonding. It is used with separately supplied Activator 7387 for room-temperature cure and can also be heat cured with the appropriate time-and-temperature schedule. With activator on one side of a steel joint, fixture is 3 minutes or less at a 0.05 mm gap. After 24 hours at 22 deg C with Activator 7387 on one side, lap shear on steel is at least 11 N/mm^2; typical cured tensile strength is 17.9 N/mm^2 and peel strength is 3.5 N/mm. Performance varies with gap, surface preparation, activator use, and cure conditions.

Key features

  • High-viscosity application control: Brookfield RVF viscosity is 75,000 to 130,000 mPa s (cP) at 25 deg C with spindle 7 at 20 rpm.
  • Fast thin-gap fixture: Fixture is 3 minutes or less at a 0.05 mm steel gap with Activator 7387.
  • Impact and peel resistance: Forms tough, durable bonds with impact and peel resistance for magnet bonding.

Applications

Structural metal-to-metal bonding, including magnet bonding and electric-motor assemblies.

Product Family

LOCTITE AA 332

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Opaque light yellow to dark amber
Chemistry TypeChemistry Type
Modified acrylic
Specific GravitySpecific Gravity
0.97
Physical Properties
ViscosityViscosity
75,000 to 130,000 mPa.s
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

The adhesive is the page entity; Activator 7387 is separately supplied and required for the cited room-temperature cure process.

PropertyValueUnitMethod / condition
AppearanceOpaque light yellow to dark amberUncured
Specific gravity0.9725 deg C
Brookfield viscosity75,000 to 130,000mPa s (cP)25 deg C; RVF; spindle 7; 20 rpm
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shore hardness69Durometer DISO 868; cured material
Tensile modulus950N/mm^2ISO 527-2; cured material
Tensile strength at break17.9N/mm^2ISO 527-2; cured material
Lap shear strength11 minimumN/mm^2Steel; 0.05 mm gap; Activator 7387 on one side; 24 h at 22 deg C
180 deg peel strength3.5N/mmISO 8510-2; steel; 24 h at 22 deg C; Activator 7387 on one side

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers