LOCTITE AA 3963

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

LOCTITE AA 3963

Main features

  • Fast Tack-Free LED Cure
  • Low-Viscosity Rigid Bonding
  • Strong Polycarbonate Assembly Bonds

Product Description

LOCTITE AA 3963 is a one-part, low-viscosity UV/visible-light-curing acrylated urethane adhesive for rigid medical-device component bonding. The transparent, fluorescent material is designed for high adhesion to metals and plastics and supports fast LED processing. On glass, fixture is achieved in 10 seconds or less with 405 nm LED light at 10 mW/cm^2; at 1,400 mW/cm^2 and 405 nm, the surface becomes tack-free in 5 to 10 seconds. After 10 seconds at 1,000 mW/cm^2 and 405 nm, typical cured properties include 23.1 N/mm^2 tensile strength and 22.7 N/mm^2 block shear on polycarbonate. Performance remains dependent on light exposure, substrate, geometry, and surface preparation.

Key features

  • Rapid tack-free LED surface cure: Tack-free time is 5 to 10 seconds at 1,400 mW/cm^2 measured at 405 nm.
  • Low-viscosity rigid bonding: Cone-and-plate viscosity is 250 to 450 mPa s (cP) at 25 deg C, measured at 100 s^-1 after 180 seconds with a Physica CP50-1 cone.
  • Polycarbonate bond strength: Typical polycarbonate-to-polycarbonate block shear is 22.7 N/mm^2 after 10 seconds at 1 W/cm^2 and 405 nm.

Applications

Bonding rigid metal and plastic components in medical-device assemblies.

Product Family

LOCTITE AA 3963

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Transparent, colorless to straw
Chemistry TypeChemistry Type
Acrylated urethane
Refractive indexRefractive index
1.5
Specific GravitySpecific Gravity
~1.02
Physical Properties
ViscosityViscosity
250 to 450 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
55 °C
Mechanical Properties
ElongationElongation
38 %
Chemical Properties
Water AbsorptionWater Absorption
6.2 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to strawUncured
UV fluorescencePositiveUnder UV light
Specific gravityApprox. 1.0225 deg C
Cone and plate viscosity250 to 450mPa s (cP)25 deg C; CP50-1; 100 s^-1; 180 s test time
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shore hardness71Durometer DISO 868; 1,000 mW/cm^2 at 405 nm for 10 s
Elongation at break38%ISO 527-3; 1,000 mW/cm^2 at 405 nm for 10 s
Tensile strength23.1N/mm^2ISO 527-3; 1,000 mW/cm^2 at 405 nm for 10 s
Glass transition temperature55deg CISO 11359-2; cured material
Polycarbonate block shear22.7N/mm^2ISO 13445; polycarbonate-to-polycarbonate; 1 W/cm^2 at 405 nm for 10 s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers