LORD 410

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LORD 410

Main features

  • 20-30 Minute Working Window
  • 0.25 mm 19GB Bondline Control
  • 4:1 Volume System Mixing

Product Description

LORD 410 is an off-white to tan acrylic adhesive component used with LORD Accelerator 19 or 19GB in a two-part structural bonding system. The adhesive component has typical viscosity of 100,000-350,000 cP at 25 deg C and density of 1,096-1,156 kg/m3. Mixed systems use a 4:1 adhesive-to-accelerator volume ratio, with a 20-30 minute working time and 60-120 minute handling-strength time at 24 deg C. Accelerator 19GB contains 0.25 mm glass spheres for bondline control; Accelerator 19 is used when thickness is controlled by other means or is greater than 0.25 mm.

Key features

  • Component Rheology: The LORD 410 adhesive component has a typical viscosity of 100,000 to 350,000 cP at 25 deg C.
  • Mixed-System Work Time: Systems mixed with Accelerator 19 or 19GB have a typical working time of 20 to 30 minutes at 24 deg C.
  • Bondline Control: Accelerator 19GB uses 0.25 mm glass spheres to control adhesive bondline thickness.

Applications

Structural bonding of engineered thermoplastics and metals within LORD 410 systems using Accelerator 19 or 19GB.

Product Family

LORD 410

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Off-white to Tan Paste
DensityDensity
1096 -1156 kg/m3
SolidsSolids
100 %
Physical Properties
ViscosityViscosity
100,000 - 300,000 mPa.s
Young's modulusYoung's modulus
896.3 MPa
Thermal Properties
Flash PointFlash Point
15 °C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
72 °C
Mechanical Properties
ElongationElongation
30 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values apply to LORD 410 adhesive component before mixing with Accelerator 19 or 19GB.

PropertyValueUnitMethod / condition
AppearanceOff-white to tan pasteTypical; LORD 410 component
Viscosity100,000-350,000cPTypical; Brookfield; 25 deg C
Density1,096-1,156kg/m3Typical; LORD 410 component
Flash point15deg CTypical
Shelf life1yearOriginal unopened container below 27 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers