LORD 810
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

Main features
- Low Read-Through Bondline
- Thin-Gauge Panel Bonding
- 2:1 Volume Mixing
Product Description
LORD 810 Low Read-Through Acrylic Adhesive is a two-component acrylic system used with LORD Accelerator 20GB for bonding thin-gauge metal and supported composite or plastic substrates. Its low-read-through formulation is intended to reduce visible bond-line distortion on appearance-sensitive panels. The system mixes at 2:1 by volume, adhesive to accelerator, using LORD 810 adhesive and Accelerator 20GB. It is suited to thin-gauge metal-to-metal assemblies and supported metal-to-composite or metal-to-plastic joints where surface appearance matters. The complete system consists of both the adhesive and accelerator, not either component alone.
Key features
- Low read-through design: Supports appearance-sensitive thin panels where visible bond-line distortion should be minimized.
- Thin-gauge substrate fit: Intended for supported metal-to-metal, metal-to-composite and metal-to-plastic bonding.
- Controlled two-component mixing: Combines LORD 810 adhesive with Accelerator 20GB at 2:1 by volume.
Applications
Applications include thin-gauge metal-to-metal bonding and supported metal-to-composite or metal-to-plastic panel assembly.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Only exact, selection-relevant system data are shown for LORD 810 with Accelerator 20GB.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Two-component low-read-through acrylic adhesive system | - | Exact LORD 810 / Accelerator 20GB page entity |
| System components | LORD 810 adhesive; LORD Accelerator 20GB | - | Part 1 and Part 2 system scope |
| Mix ratio | 2:1 | parts by volume | LORD 810 adhesive to Accelerator 20GB |