PERMABOND HM161

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

PERMABOND HM161

Main features

  • Slip-Fit Cylindrical Retention with 0.25 mm Gap Fill
  • Fast Slip-Fit Assembly Handling
  • High-Shear Retention for Mated Metal Parts

Product Description

Permabond HM161 is a one-part anaerobic retaining compound for cylindrical metal parts and slip-fit assemblies. The liquid cures when confined between mating metal surfaces, unitizing the parts and limiting relative movement that can contribute to wear, erosion and pitting. It fills gaps up to 0.25 mm and reaches typical handling strength on M10 steel in 10 minutes at 23 deg C. After cure, HM161 develops typical 24 MPa shear strength on a steel collar-and-pin test to ISO 10123. Its 2,000 cP viscosity balances gap filling with a liquid application profile for cylindrical retention.

Key features

  • Slip-fit cylindrical retention: Retains mated cylindrical metal parts and slip-fit assemblies.
  • 0.25 mm gap fill: Fills gaps up to 0.25 mm between mating metal parts.
  • High cured shear strength: Typical shear strength is 24 MPa on a steel collar-and-pin test to ISO 10123.

Applications

Retaining cylindrical metal parts; slip-fit assemblies; prevention of movement, wear and corrosion between mated metal parts.

Product Family

PERMABOND HM161

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Green
Chemistry TypeChemistry Type
Methacrylates
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
2000 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
11 kV/mm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.2 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionMethacrylates-Uncured material
Viscosity2,000cPUncured material; 25 deg C
Specific gravity1.1-Uncured material
Storage temperature5 to 25deg CManufacturer storage guidance
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Break torque31N mTypical cured material; M10 steel; ISO 10964
Prevailing torque45N mTypical cured material; M10 steel; ISO 10964
Shear strength24MPaTypical cured material; steel collar and pin; ISO 10123

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers