PERMABOND TA4820

Main features

  • Extended 10-15 Minute Pot Life
  • Thixotropic 2 mm Gap Filling
  • High Peel Strength with Cured Elongation

Product Description

Permabond TA4820 is a two-component 1:1 toughened methacrylate structural adhesive for thermoplastics, thermosets, metals and composites. At 23 deg C, pot life is 10-15 minutes, fixture time is 25-35 minutes and handling strength is reached in 45-60 minutes. The thixotropic adhesive fills gaps up to 2 mm and can be dispensed through a static mixer. After cure, typical lap-shear strength is 21-28 N/mm2 on steel and 17-24 N/mm2 on aluminum. Typical peel strength is 70-90 N/25 mm, and cured elongation is 15-20%.

Key features

  • 10-15 minute pot life: Pot life is 10-15 minutes at 23 deg C, followed by 25-35 minute fixture time.
  • Thixotropic 2 mm gap filling: The 1:1 adhesive fills gaps up to 2 mm and can be dispensed through a static mixer.
  • Peel strength with cured elongation: Typical peel strength is 70-90 N/25 mm to ISO 4578 and cured elongation is 15-20% to ISO 37.

Applications

Structural bonding of thermoplastics, thermosets, metals and composites.

Product Family

PERMABOND TA4820

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Off-white/Amber
Chemistry TypeChemistry Type
Methyl methacrylate
Specific GravitySpecific Gravity
1.0
Physical Properties
ViscosityViscosity
200,000-300,000/120,000-200,000 mPa.s
Mechanical Properties
ElongationElongation
15 - 20 %
Electrical Properties
Dielectric StrengthDielectric Strength
30-50 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part A viscosity200,000-300,000cP25 deg C
Part B viscosity120,000-200,000cP25 deg C
Mix ratio1:1-Part A : Part B
Maximum gap fill2mmMixed adhesive
Pot life10-15min10 g + 10 g mixed mass; 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Lap-shear strength21-28N/mm2Typical cured joint; steel; ISO 4587
Lap-shear strength17-24N/mm2Typical cured joint; aluminum; ISO 4587
Peel strength70-90N/25 mmTypical cured joint; ISO 4578
Tensile strength29N/mm2Typical cured adhesive; ISO 37
Elongation15-20%Typical cured adhesive; ISO 37

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers