PERMABOND UV643

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV643

Main features

  • Sub-Second High-Intensity Fixture
  • Thixotropic Rigid-Plastic Bonding
  • Hot-Wet Strength Retention

Product Description

Permabond UV643 is a thixotropic, extremely fast urethane-acrylate adhesive for UV bonding of rigid plastics and metal-to-plastic assemblies. It cures tack-free across 365 to 420 nm and bonds polycarbonate, PMMA, PETG, PET, ABS, and rigid PVC under the specified process conditions. Typical fixture time is under 1 second with the listed 330 mW/cm^2 mercury lamp or 400 nm, 150 mW/cm^2 LED, and 19 seconds at 0.1 mW/cm^2. Cured data include 23 N/mm^2 tensile strength, 50% elongation, and retained polycarbonate shear strength after four weeks at 85 deg C and 85% RH.

Key features

  • Thixotropic Application Control: Viscosity is 2,000 mPa s at 20 rpm and 17,600 mPa s at 2 rpm.
  • Sub-Second High-Intensity Fixture: Typical fixture time is under 1 second with the listed high-intensity UV lamp conditions.
  • Hot-Wet Strength Retention: Polycarbonate shear strength remained 13 N/mm^2 after four weeks at 85 deg C and 85% RH.

Applications

Applications include fast bonding of PC, PMMA, PETG, PET, ABS, rigid PVC, and supported metal-to-plastic combinations.

Product Family

PERMABOND UV643

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionUrethane acrylateAs supplied
AppearancePale yellowColorless when cured
Viscosity2,000mPa sAt 25 deg C; 20 rpm
Viscosity17,600mPa sAt 25 deg C; 2 rpm
Specific gravity1.0As supplied
Typical fixture time<1 to 19secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Overlap shear strength - polycarbonate13N/mm^2Substrate failure observed
Overlap shear strength - acrylic7N/mm^2Typical cured value
Overlap shear strength - aluminum to PC10N/mm^2Typical cured value
Tensile strength23N/mm^2ASTM D638
Elongation at break50%ASTM D638
Elastic modulus1.2GPaASTM D638
Hardness65Shore DISO 868
Polycarbonate shear after hot-wet aging13N/mm^24 weeks at 85 deg C and 85% RH; tested at 23 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers