PLEXUS MA205HV

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

PLEXUS MA205HV

Main features

  • Non-Conductive Electronic Structural Bonding
  • 3-5 Minute Work Time
  • 15.9 MPa Aluminum Lap Shear

Product Description

Plexus MA205HV is a non-conductive two-part 10:1 methacrylate structural adhesive for electronic assemblies, metals, engineered thermoplastics and composites. At 23.9 deg C, typical work time is 3-5 minutes, and the adhesive reaches 50 psi handling strength in about 7-8 minutes on polycarbonate. The thixotropic system fills gaps from 0.75 to 6.4 mm. After cure, typical tensile strength is 13.7-16.7 MPa, elongation at break is 15-30%, and aluminum lap-shear strength is 15.9 MPa. Primerless metal bonding is supported for manufacturer-listed substrates.

Key features

  • Non-conductive structural bonding: The adhesive is positioned for structural electronic assemblies as well as supported metals, thermoplastics and composites.
  • 3-5 minute work time: Typical work time is 3-5 minutes at 23.9 deg C, with 50 psi handling strength in about 7-8 minutes on polycarbonate.
  • 15.9 MPa aluminum lap shear: Typical aluminum lap-shear strength is 15.9 MPa to ASTM D1002.

Applications

Structural bonding of electronic assemblies; primerless bonding of supported metals; bonding engineered thermoplastics and composites.

Product Family

PLEXUS MA205HV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White/Blue
Density (g)Density (g)
0.96/1.07 g/cm3
Mix RatioMix Ratio
10:1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
100 - 130 mPa.s
Viscosity (Part B)Viscosity (Part B)
15 - 50 mPa.s
Mechanical Properties
ElongationElongation
15 - 30 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part A viscosity100,000-130,000cPUncured adhesive
Part B viscosity15,000-50,000cPUncured activator
Part A density0.96g/mlUncured adhesive
Part B density1.07g/mlUncured activator
Mix ratio by volume10:1-Part A : Part B
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile strength13.7-16.7MPaTypical cured adhesive; ASTM D638 / ISO 527
Tensile modulus996-1,348MPaTypical cured adhesive; ASTM D638 / ISO 527
Elongation at break15-30%Typical cured adhesive; ASTM D638 / ISO 527
Lap-shear strength15.9MPaTypical cured joint; aluminum; ASTM D1002

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers