PLEXUS MA2090

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

PLEXUS MA2090

Main features

  • Highly Thixotropic Vertical-Bead Control
  • 90-95 Minute Work Time
  • 0.75-38 mm Non-Sag Gap Filling

Product Description

Plexus MA2090 is a highly thixotropic two-part 10:1 methacrylate structural adhesive for composite, thermoplastic and metal assemblies. The non-sagging formulation resists bead sag and slide on vertical surfaces. At 23.9 deg C, typical work time is 90-95 minutes, supporting large assemblies that require extended positioning time. The adhesive fills gaps from 0.75 to 38 mm. After cure, typical tensile strength is 15.2-20.0 MPa, elongation at break is 90-120%, and aluminum lap-shear strength is 12.4 MPa.

Key features

  • Highly thixotropic vertical-bead control: The formulation is designed to resist adhesive sag and slide on vertical surfaces.
  • 90-95 minute work time: Typical work time is 90-95 minutes at 23.9 deg C.
  • Non-sag gap filling to 38 mm: The adhesive is specified for gaps from 0.75 to 38 mm.

Applications

Structural bonding of composites, thermoplastics and metals; vertical bonding; large-bead assemblies requiring extended working time.

Product Family

PLEXUS MA2090

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White/(Blue/Black)
Density (g)Density (g)
0.94/1.07 g/cm3
Mix RatioMix Ratio
10:1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
180 - 220 mPa.s
Viscosity (Part B)Viscosity (Part B)
35 - 70 mPa.s
Mechanical Properties
ElongationElongation
90 - 120 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part A viscosity180,000-220,000cPUncured adhesive
Part B viscosity35,000-70,000cPUncured activator
Part A density0.94g/mlUncured adhesive
Part B density1.07g/mlUncured activator
Mix ratio by volume10:1-Part A : Part B
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile strength15.2-20.0MPaTypical cured adhesive; ISO 527
Tensile modulus413-689MPaTypical cured adhesive; ISO 527
Elongation at break90-120%Typical cured adhesive; ISO 527
Lap-shear strength12.4MPaTypical cured joint; aluminum; ASTM D1002

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers