- Rapid 1-2 Minute Work Window
- Controlled 1-4 mm Gap Range
- Robotic Plastic Assembly Fit
Product Description
Plexus MA420FS is a two-part, 10:1 methacrylate adhesive for fast structural assembly of thermoplastics, metals, and composites. Its 1-2 minute work time supports short-cycle part placement, while the 1-4 mm gap range accommodates defined plastic-component joint geometries. The grade is intended for robotic or automated assembly where a controlled mix ratio and rapid processing are required. Applications include fast structural bonding of plastic components and other supported thermoplastic, metal, and composite assemblies.
Key features
- 1-2 Minute Work Window: Supports short-cycle adhesive application and part placement.
- 1-4 mm Gap Range: Supports structural plastic-assembly joints within the stated range.
- Automated Assembly Fit: Supports robotic or automated plastic-component assembly.
Applications
Applications include rapid structural assembly of plastic components and supported thermoplastic, metal, and composite assemblies.
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| System form | Two-part methacrylate adhesive | As supplied | |
| Mix ratio by volume | 10:1 | Adhesive to activator | |
| Work time | 1-2 | minutes | Typical processing value |
| Gap range | 1-4 | mm | Typical joint range |