Thermal Putty pads

High Compressibility and Thermal Conductivity

Thermal putty pads

Thermally Conductive Putty Pads provide high thermal performance and solid thermal reliability. The material’s putty-like consistency enables excellent gap-filling capability for applications with large dimensional variances.

Special surface reinforcement enables easier handling for operators, with no pull-out during high-volume assembly. The product is naturally tacky and requires no additional adhesive to mate to the heat source and heat sink. Putty pads combine ultra soft - high compressibility with a low surface impedance that is complemented by natural tackiness and ease of application.

Typical applications for putty pads can be found in EV battery & charging stations, automotive electronics, power devices & modules, telecommunications & network servers.

Thermal putty pads are available in thicknesses ranging from 0.5mm to 5.0mm.

4 products

  • HGP12PT | High Thermal Conductivity Putty Pad

    HGP12PT | High Thermal Conductivity Putty Pad

    • 0.13 Thermal Impedance
    • 12 Thermal Conductivity
    • Low oil bleeding & Low volatile
  • LAIRD TPUTTY 607

    LAIRD TPUTTY 607

    • 6.4 W/(m K) Thermal Interface
    • No-Mix Thermal Interface Processing
    • Automation-Oriented Dispensing and Vertical Stability
  • LAIRD TPUTTY 502FG2

    LAIRD TPUTTY 502FG2

    • 3.0 W/(m K) Thermal Interface
    • Ultra-Soft 14 Shore 00 Material
    • Thermal Interface Material
  • LAIRD TPUTTY 508

    LAIRD TPUTTY 508

    • One-Part Automated Dispensing
    • Vertical Gap-Filler Stability
    • 3.7 W/(m K) Thermal Transfer

Product selector guide

Thermal Putty Pads
Product name Color Thickness (mm)1 Hardness (Shore00) Specific Gravity Thermal Conductivity (W/m·K) Thermal Impedance(˚C·in2/W)(1mm@10psi) Dielectric Constant @1MHz Volume Resistivity (ohm·cm) Flammability Rating
TGP 3500PT Green 0.5-5 5 3.2 3.5 0.45 6.4 4.0 x 1013 V-0
TGP 3510PT Green 0.5-5 5 3.2 3.5 0.45 6.4 4.0 x 1013 V-0
TGP 6000PT Grey 0.5-5 5 3.4 6.0 0.27 6.5 4.0 x 1015 V-0
TGP 8000PT Grey 0.5-5 5 3.5 8.0 0.19 8.5 4.0 x 1015 V-0

Frequently asked questions

What are the benefits of Thermal putty pads?

The material’s putty like design makes it ultra soft and compressible and enables excellent gap filling capability for applications with large dimensional variances. Special surface reinforcement enables easier handling for operators during high volume assembly.

The hardness is completely different compared to gap pads. Putties are soft and require little to no pressure, something that makes them good replacements for thermal gels. They are non electrically conductive and come in large form factors they work great if properly handled.

Additionally, they are naturally tacky and require no additional adhesive to mate the heat source and heat sink.

What are some typical Thermal putty pad applications?

Typical Thermal Grease Applications include:

  • EV Battery & Charging stations
  • Automotive electronics
  • Power devices and modules
  • Telecommunication & network servers

This product is for the applications which are sensitive to assembly pressure. That's why the mechanical strength of this pad is limited. 


Do putty pads provide electrical insulation?

Putty pads use non-electrically conductive thermal fillers, giving them naturally high dielectric strength typically around 5 kV/mm. However, dielectric strength is not listed in the TDS because these materials are designed primarily for thermal management, not as the main electrical-insulation barrier. The actual dielectric performance of any putty pad also depends on coating quality and material integrity, even a small internal void can significantly reduce insulation capability. For applications requiring guaranteed electrical isolation, a dedicated insulation material should still be used.


Learn more

Thermal Putty Pads

Thermal putty pads are thermal interface materials that are soft and pliable. While their function is similar with thermal gap pads, thermal putty pads are typically used in applications with uneven surfaces or or irregular geometries that require flexible gap-filling.

Thermal Putty Pads V.S. Thermal Gap Pad

Standard thermal gap pad materials have tensile strength, but little elasticity. Standard gap pads and putty gap pads have essentially the same performance for a given gap. The compression behaviour differences are as follows:

No Tensile Strength Compresses Down Significantly

Putty pads don't have tensile strength and elasticity

  • Putty pads require a minimum amount of compression; at least 10%. They are soft, and eventually they will bottom out past 80%. 
  • They also relax over time. what’s referred to as densification. The material is no longer flowing and is being crushed. Make sure not to exceed a certain amount of force when using these materials.

Putty pads compress significantly

  • Thermal putty pads can be pulled apart very easily and are applied in the same manner as a gap filler pad. The compression is 100%.
  • They do not bounce back. It’s important to ensure two good surfaces that will not move if using putty pads.

Stress Of Thermal Putty Pad

Putty pads are ultra-soft

Thermal putty pads and thermal gap pad are similar products. For example, TGP8000 and TGP8000PT both have high thermal conductivity as 8 W/m.K and need at least 10% compression while applying. The main difference is that thermal putty pads are ultra-soft and could be compressed up to 90%. It almost has no tensile strength and no elasticity, thus will not recover and bounce back. Due to the low stress and high compressibility, thermal putty pads are more suitable for applications with large dimensional variances, comparing with traditional thermal gap pad. 

Difference with thermal gels

Both thermal putty pad and thermal hybrid gel belong to gap filler type TIM, which are applicable for large bond line thickness application (>0.5mm). Thermal gel products are designed for automation process such as dispensing. Compared with hybrid gels, putty pads are suitable for large area assembly. It is easy to apply thermal putty pads manually and there is no need for dispensing equipment. 


putty pads vs gap pads


Related Blogs

PCM101


Phase change materials 101

This blog discusses the fundamentals of phase change materials.

SivsSiFree


Si vs Si-Free TIMs

This blog discusses the differences between thermal interface materials with and without silicones.

TIMsAndDataCenters


TIMs and Data Centers

This blog explores how TIMs play a role in enhancing efficiency of big data centers and high power computing.


Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers